化工进展 ›› 2023, Vol. 42 ›› Issue (8): 4458-4464.DOI: 10.16085/j.issn.1000-6613.2022-1738

• 资源与环境化工 • 上一篇    

亲水和疏水改性膜的抗结垢和润湿能力的对比

李雪佳1(), 李鹏1, 李志霞2, 晋墩尚2, 郭强3,4, 宋旭锋2, 宋芃2, 彭跃莲2()   

  1. 1.国能神东煤炭集团有限责任公司煤炭开采水资源保护与利用国家重点实验室,陕西 榆林 719315
    2.北京工业大学环境与生命学部,北京 100124
    3.北京低碳清洁能源研究院,北京 101303
    4.煤炭开采水资源保护与利用国家重点实验室,北京 102208
  • 收稿日期:2022-09-19 修回日期:2022-11-17 出版日期:2023-08-15 发布日期:2023-09-19
  • 通讯作者: 彭跃莲
  • 作者简介:李雪佳(1986―),男,高级工程师,研究方向为煤炭开采。E-mail:541207880@qq.com
  • 基金资助:
    国家自然科学基金(21878005);国能神东煤炭集团有限责任公司煤炭开采水资源保护与利用国家重点实验室(WPUKFJJ2019-13)

Experimental comparation on anti-scaling and anti-wetting ability of hydrophilic and hydrophobic modified membranes

LI Xuejia1(), LI Peng1, LI Zhixia2, JIN Dunshang2, GUO Qiang3,4, SONG Xufeng2, SONG Peng2, PENG Yuelian2()   

  1. 1.State Key Laboratory of Water Resource Protection and Utilization in Coal Mining, CHN Energy Shendong Coal Group Co. , Ltd. , Yulin 719315, Shaanxi, China
    2.Faculty of Environment and Life, Beijing University of Technology, Beijing 100124, China
    3.National Institute of Clean-and-Low-Carbon Energy, Beijing 101303, China
    4.State Key Laboratory of Water Resource Protection and Utilization in Coal Mining, Beijing 102208, China
  • Received:2022-09-19 Revised:2022-11-17 Online:2023-08-15 Published:2023-09-19
  • Contact: PENG Yuelian

摘要:

膜蒸馏过程受料液盐度的影响较小,可以处理高矿化度的矿井水,但膜污染和润湿制约其工业化应用。本文首次全面比较了两种商业化的疏水膜,即平板聚四氟乙烯(PTFE)和聚偏氟乙烯(PVDF),以及分别进行亲水和疏水表面改性后制备的PVA-PAA/PTFE和Teflon/PVDF两种复合膜,在直接接触式膜蒸馏(DCMD)中浓缩饱和硫酸钙溶液时的结垢和润湿程度。重点分析了两种基膜和复合膜的结垢和润湿机理,探讨它们在矿井水浓缩中的应用潜力和最佳膜结构。实验结果显示,饱和硫酸钙浓缩过程中,膜表面结垢是主要影响因素,PTFE膜和PVDF膜尽管膜微观结构差别巨大,但抗结垢能力接近;Teflon/PVDF复合膜因其表面有滑移特性而表现出完美的抗结垢性能,PVA-PAA/PTFE复合膜尽管有致密的亲水表面,抗结垢能力并不强。

关键词: 矿井水, 膜蒸馏, 亲水改性, 疏水改性, 结垢, 润湿

Abstract:

Membrane distillation processes are less affected by water with high salinity, including high saline water from mines. However, membrane scaling and wetting have restricted their industrial applications. In this work, we compared two types of commercial flat hydrophobic membranes, i.e., polytetrafluoroethylene (PTFE) and polyvinylidene fluoride (PVDF), with their composite membranes. The composite membranes were prepared with hydrophilic and hydrophobic surface modification, namely PVA-PAA/PTFE and Teflon/PVDF. The effects of membrane scaling and wetting on the prepared membranes were systematically investigated using the concentrated saturated calcium sulfate (CaSO4) solution in direct contact membrane distillation (DCMD). We analyzed their membrane scaling and wetting mechanisms and presented their potential application and optimal membrane structure for high-saline mine water. Our experimental results indicated that the scaling on the membrane surface was the main influencing factor in the concentration process of the CaSO4 solution in DCMD. Although the microstructures of the bare and modified membranes differed, their anti-scaling abilities were similar. Compared to the other prepared membranes, the Teflon/PVDF composite membrane exhibited superior anti-scaling performance given its slip characteristics. On the other hand, the PVA-PAA/PTFE composite membrane exhibited marginal improvement in anti-scaling ability despite its dense hydrophilic surface.

Key words: high-saline mine water, membrane distillation, hydrophilic surface modification, hydrophobic surface modification, scaling, wetting

中图分类号: 

京ICP备12046843号-2;京公网安备 11010102001994号
版权所有 © 《化工进展》编辑部
地址:北京市东城区青年湖南街13号 邮编:100011
电子信箱:hgjz@cip.com.cn
本系统由北京玛格泰克科技发展有限公司设计开发 技术支持:support@magtech.com.cn