Chemical Industry and Engineering Progress ›› 2017, Vol. 36 ›› Issue (S1): 572-577.DOI: 10.16085/j.issn.1000-6613.2017-2236

Previous Articles     Next Articles

Crosslinking modification of feather keratin/sodium alginate blend films

HE Ming1, DOU Yao1, YIN Guoqiang2, CUI Yingde1,3   

  1. 1. School of Material Science and Engineering, Northwestern Polytechnical University, Xi'an 710072, Shaanxi, China;
    2. College of Chemistry and Chemical Engineering, Zhongkai University of Agriculture and Engineering, Guangzhou 510225, Guangdong, China;
    3. Guangzhou Vocational College of Science and Technology, Guangzhou 510550, Guangdong, China
  • Received:2017-10-27 Online:2017-12-13 Published:2017-12-31

羽毛角蛋白/海藻酸钠共混膜的交联改性

何明1, 窦瑶1, 尹国强2, 崔英德1,3   

  1. 1. 西北工业大学材料学院, 陕西 西安 710072;
    2. 仲恺农业工程学院化学化工学院, 广东 广州 510225;
    3. 广州科技职业技术学院, 广东 广州 510550
  • 通讯作者: 尹国强,教授。
  • 作者简介:何明(1984-),男,博士研究生。E-mail:heming1026@163.com。
  • 基金资助:
    国家自然科学基金(21176269)、广东省自然科学基金(2016A030313371)及广州市科技计划(201704030130)项目。

Abstract: Crosslinked and sorbitol-plasticized feather keratin (FK)/sodium alginate (SA) blend films were prepared by the casting process, using glyoxal, glutaraldehyde, or alginate dialdehyde (ADA) as crosslinker. The effects of crosslinking modification on the structure and properties of the blend films were investigated. FTIR analysis confirmed the crosslinking reaction in the process of modification. SEM results showed that crosslinking made the microstructure of the blend films more compact. After crosslinking, the thermal stability and moisture resistance of the blend films were enhanced, the transmittance and the elongation at break decreased. The tensile strength increased when crosslinked with glyoxal or glutaraldehyde, and decreased when crosslinked with ADA.

Key words: feather, keratin, protein films, blends, crosslinking

摘要: 以山梨醇为增塑剂,乙二醛、戊二醛或自制的双醛海藻酸钠(ADA)为交联剂,采用浇铸法制备了交联改性的羽毛角蛋白(FK)/海藻酸钠(SA)共混膜,研究了交联改性对共混膜结构和性能的影响。FTIR分析证实了交联反应的发生,SEM结果表明,经过交联改性的共混膜内部结构更加致密。性能测试结果表明,交联改性后共混膜的热稳定性和阻湿性增强,透光性减弱,断裂伸长率减小。乙二醛、戊二醛交联时膜的抗拉强度增加,ADA交联时膜的抗拉强度减小。

关键词: 羽毛, 角蛋白, 蛋白膜, 共混, 交联